Estudo da produção de concentrados de minério de ferro a partir dos rejeitos da barragem de germano.
dc.contributor.advisor | Martins, Jader | pt_BR |
dc.contributor.author | Santos, Ivan José dos | |
dc.contributor.referee | Peres, Antônio Eduardo Clark | pt_BR |
dc.contributor.referee | Donda, Joaquim Donizetti | pt_BR |
dc.contributor.referee | Martins, Jader | pt_BR |
dc.date.accessioned | 2019-03-18T16:08:05Z | |
dc.date.available | 2019-03-18T16:08:05Z | |
dc.date.issued | 2003 | |
dc.description | Programa de Pós-Graduação em Engenharia Mineral. Departamento de Engenharia de Minas, Escola de Minas, Universidade Federal de Ouro Preto. | pt_BR |
dc.description.abstract | Esse trabalho investigou a possibilidade de se produzir concentrados de minério de ferro que atendessem às especificações atuais da Samarco, utilizando uma amostra dos rejeitos da barragem de Germano. Na caracterização da amostra, determinou-se uma granulometria muito fina, um baixo teor de ferro (26%) e um elevado teor de hematita especular (85%), além de uma maior concentração dos minerais de ferro nas frações abaixo de 44m. Devido a essas características, foram realizados inicialmente ensaios de pré-concentração por peneiramento, concentração magnética e concentração centrífuga. Na seqüência, foram realizados ensaios de concentração considerando cinco fluxogramas, envolvendo como métodos principais a concentração magnética e a flotação. Os concentrados obtidos apresentaram baixos teores de fósforo, elevados teores de hematita especular e teores de sílica próximos às especificações de alto forno. A especificação de sílica de um concentrado para redução direta não foi prontamente obtida e mostrou-se mais difícil, fato atribuído à presença no concentrado de outras espécies portadoras de sílica, além do quartzo. Os fluxogramas envolvendo peneiramento e concentração magnética foram os que se mostraram mais promissores para o tratamento dos rejeitos. Mesmo sem otimizações, foram obtidas recuperações em peso de 25% e metálica de 67%, com teores de sílica no concentrado na faixa de 3%. Por possuir configuração semelhante ao circuito de concentração da Samarco, a opção incluindo deslamagem e flotação foi melhor estudada através de um projeto de experimentos para os ensaios de flotação e também considerando a introdução de uma etapa de escrubagem anterior à deslamagem. Os resultados obtidos não recomendam a utilização desse tipo de circuito para o tratamento dos rejeitos da barragem de Germano. | pt_BR |
dc.description.abstracten | This research investigated the possibilities of producing iron ore concentrates in accordance with the specifications of the concentrates produced by Samarco, using a sample of Germano´s tailings dam. The sample characterization determined a very fine size distribution, a low iron grade (26%) and a high specular hematite content (85%), beyond a high concentration of iron minerals in fractions below 44m. Due to these characteristics, pre-concentration tests using screening, magnetic and and centrifugal concentration were carried out first. Following, concentration tests were carried out considering five flowsheets, considering flotation and magnetic concentration as major methods. The concentrates obtained showed a low phosphorous grade, a high specular hematite content and silica grades close to the blast furnace specifications. The silica specification for direct reduction wasn’t readily achieved, and seemed to be more difficult to be, fact attributed to others mineral species containing silica, different from quartz, found in the concentrates. The flowsheets using screening and magnetic concentration were the most promissory to treat the tailings. Even without optimization, weight and iron recoveries of 25 and 67% were obtained, and concentrates with silica grades around 3%. Due to its similarity with Samarco´s concentration flowsheet, the option with desliming and flotation was better studied using a design of experiments for flotation tests and also considering a scrubbing stage before desliming. The results obtained don´t recommend this flowsheet to the treatment of the tailings of Germano´s dam. | pt_BR |
dc.identifier.citation | SANTOS, Ivan José dos. Estudo da produção de concentrados de minério de ferro a partir dos rejeitos da barragem de germano. 2003. 103 f. Dissertação (Mestrado em Engenharia Mineral) - Escola de Minas, Universidade Federal de Ouro Preto, Ouro Preto, 2003 | pt_BR |
dc.identifier.uri | http://www.repositorio.ufop.br/handle/123456789/10804 | |
dc.language.iso | pt_BR | pt_BR |
dc.rights | aberto | pt_BR |
dc.rights.license | Autorização concedida ao Repositório Institucional da UFOP pelo(a) autor(a) em 13/03/2019 com as seguintes condições: disponível sob Licença Creative Commons 4.0 que permite copiar, distribuir e transmitir o trabalho desde que sejam citados o autor e o licenciante. Não permite o uso para fins comerciais nem a adaptação. | pt_BR |
dc.subject | Rejeitos | pt_BR |
dc.subject | Minério de ferro | pt_BR |
dc.subject | Concentração | pt_BR |
dc.title | Estudo da produção de concentrados de minério de ferro a partir dos rejeitos da barragem de germano. | pt_BR |
dc.type | Dissertacao | pt_BR |
Files
Original bundle
1 - 1 of 1
No Thumbnail Available
- Name:
- DISSERTAÇÃO_EstudoProduçãoConcentrados.pdf
- Size:
- 2.86 MB
- Format:
- Adobe Portable Document Format
License bundle
1 - 1 of 1
No Thumbnail Available
- Name:
- license.txt
- Size:
- 924 B
- Format:
- Item-specific license agreed upon to submission
- Description: